Decreasing the cycle time to about 20 seconds by setting a constant mold temperatre in whole cycle of hot embossing.

Featured Image

Why is it important?

Properly select the embossing windows

Perspectives

May be used for fabricate light guide plate, microneedles and so on

Professor Daming Wu
Beijing University of Chemical Technology

Read the Original

This page is a summary of: Rapid fabrication of microstructure on PMMA substrate by the plate to plate Transition-Spanning isothermal hot embossing method nearby glass transition temperature, Polymer Engineering & Science, August 2016, Wiley,