What is it about?

Stainless steel (316L) in the as-printed state is susceptible to localized attack at the boundaries of the melt pools.

Featured Image

Why is it important?

Applications of this material would usually not involve any heat treatment before use, so this susceptibility could lead to corrosion failures of parts made from it.

Perspectives

Writing this paper has allowed the authors to establish a strong collaboration that leverages our individual strengths in order to address complex issues.

Rob Kelly
University of Virginia

Read the Original

This page is a summary of: Unexpected Interface Corrosion and Sensitization Susceptibility in Additively Manufactured Austenitic Stainless Steel, CORROSION, February 2018, NACE International,