The PEDOT:PSS/SWCNT composite films with excellent thermoelectric properties could be fabricated by just mixing their water dispersion and washing the film to remove the surfactant.
Featured Image
Why is it important?
The fabrication method is quite simple; (1) just mixing the commercially available water dispersion of poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate) (PEDOT:PSS) and single-wall carbon nanotube (SWCNT); (2) removal of surfactant, which was originally contained in SWCNT dispersion, by just dipping the film for only 2 minutes. The ZT value of the composite film was around 0.1.
Perspectives
Read the Original
This page is a summary of: Highly improved thermoelectric performances of PEDOT:PSS/SWCNT composites by solvent treatment, Organic Electronics, December 2017, Elsevier,