The initial crack length (a i) was assumed to be equal to 0.1 mm in case of weld toe. This length was satisfactory for different butt joints geometries.
Featured Image
Why is it important?
Determine the initial crack length that influence on fatigue life. Also, Benchmarking result has been presented.
Perspectives
Read the Original
This page is a summary of: The Effect of Weld Profile and Geometries of Butt Weld Joints on Fatigue Life Under Cyclic Tensile Loading, Journal of Materials Engineering and Performance, October 2010, Springer Science + Business Media,
DOI: 10.1007/s11665-010-9775-1.