All Stories

  1. Quasicrystalline Composites by Additive Manufacturing
  2. Mechanism of formation of fibrous eutectic Si and thermal conductivity of SiC p /Al-20Si composites solidified under high pressure
  3. Corrosion properties of high-strength nanocrystalline Al 84 Ni 7 Gd 6 Co 3 alloy produced by hot pressing of metallic glass
  4. Formation of metastable cellular microstructures in selective laser melted alloys
  5. Selective laser melting of Al-Zn-Mg-Cu: Heat treatment, microstructure and mechanical properties
  6. Designing a novel functional-structural NiTi/hydroxyapatite composite with enhanced mechanical properties and high bioactivity
  7. Effect of Si content on the microstructure and properties of Al–Si alloys fabricated using hot extrusion
  8. Is the energy density a reliable parameter for materials synthesis by selective laser melting?
  9. Defining the tensile properties of Al-12Si parts produced by selective laser melting
  10. Microstructure and thermal expansion behavior of Al-50Si synthesized by selective laser melting
  11. Rapid fabrication of function-structure-integrated NiTi alloys: Towards a combination of excellent superelasticity and favorable bioactivity
  12. Compression behavior of inter-particle regions in high-strength Al84Ni7Gd6Co3 alloy
  13. Effect of high pressure solidification on tensile properties and strengthening mechanisms of Al-20Si
  14. Evaluation of mechanical and wear properties of Ti xNb 7Fe alloys designed for biomedical applications
  15. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting
  16. Kinetic analysis of the non-isothermal crystallization process, magnetic and mechanical properties of FeCoBSiNb and FeCoBSiNbCu bulk metallic glasses
  17. Microstructure and phase formation in Al–20Si–5Fe–3Cu–1Mg synthesized by selective laser melting
  18. Fabrication of Fe-based bulk metallic glass by selective laser melting: A parameter study
  19. Hybrid nanostructured aluminum alloy with super-high strength
  20. Influence of milling time on microstructure and magnetic properties of Fe80P11C9 alloy produced by mechanical alloying
  21. Processing of Al–12Si–TNM composites by selective laser melting and evaluation of compressive and wear properties
  22. Additive manufacturing of Cu–10Sn bronze
  23. Effect of Powder Particle Shape on the Properties of In Situ Ti–TiB Composite Materials Produced by Selective Laser Melting
  24. Length scale-dependent structural relaxation in Zr 57.5 Ti 7.5 Nb 5 Cu 12.5 Ni 10 Al 7.5 metallic glass
  25. Evolution of microstructure and mechanical properties of as-cast Al-50Si alloy due to heat treatment and P modifier content
  26. Tensile properties of Al–12Si matrix composites reinforced with Ti–Al-based particles
  27. Effect of Milling Time and the Consolidation Process on the Properties of Al Matrix Composites Reinforced with Fe-Based Glassy Particles
  28. Selective Laser Melting of Ti-45Nb Alloy
  29. Production of high strength Al85Nd8Ni5Co2 alloy by selective laser melting
  30. Comparison of wear properties of commercially pure titanium prepared by selective laser melting and casting processes
  31. Mechanical behavior of porous commercially pure Ti and Ti–TiB composite materials manufactured by selective laser melting
  32. Microstructure and mechanical properties of Mg–Al-based alloy modified with cerium
  33. The thermal expansion behaviour of SiCp/Al–20Si composites solidified under high pressures
  34. Al-based metal matrix composites reinforced with Fe49.9Co35.1Nb7.7B4.5Si2.8 glassy powder: Mechanical behavior under tensile loading
  35. High-strength ultrafine grain Mg–7.4%Al alloy synthesized by consolidation of mechanically alloyed powders
  36. Tribological and corrosion properties of Al–12Si produced by selective laser melting
  37. Friction welding of Al–12Si parts produced by selective laser melting
  38. Fabrication and mechanical properties of Al-based metal matrix composites reinforced with Mg65Cu20Zn5Y10 metallic glass particles
  39. Effect of ball milling on structure and thermal stability of Al84Gd6Ni7Co3 glassy powders
  40. Mechanical behavior of Al-based matrix composites reinforced with Mg58Cu28.5Gd11Ag2.5 metallic glasses
  41. Tensile properties of Al matrix composites reinforced with in situ devitrified Al84Gd6Ni7Co3 glassy particles
  42. Influence of Annealing on Mechanical Properties of Al-20Si Processed by Selective Laser Melting
  43. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment
  44. Production of Porous β-Type Ti–40Nb Alloy for Biomedical Applications: Comparison of Selective Laser Melting and Hot Pressing
  45. Microstructure and magnetic properties of soft magnetic composites based on silicon resin coated Co40Fe22Ta8B30 glassy powders
  46. Fabrication and characterization of bulk glassy Co40Fe22Ta8B30 alloy with high thermal stability and excellent soft magnetic properties
  47. Production of customized hybrid porous structures by powder metallurgy of Ni59Zr20Ti16Si2Sn3 glassy powders
  48. Synthesis and Characterization of NanocrystallineMg-7.4%Al Powders Produced by Mechanical Alloying
  49. Mechanical behavior of the cold-rolled Zr57Ti8Nb2.5Cu13.9Ni11.1Al7.5metallic glass–quasicrystalline composite
  50. Modeling the strengthening effect of Al–Cu–Fe quasicrystalline particles in Al-based metal matrix composites
  51. Phase transitions in Al3Ca8 and Al14Ca13 intermetallic compounds induced by milling and annealing
  52. Structural and Mechanical Characterization of Zr58.5Ti8.2Cu14.2Ni11.4Al7.7 Bulk Metallic Glass
  53. Fabrication and Response of Al70Y16Ni10Co4Glass Reinforced Metal Matrix Composites
  54. Comment on the paper ‘Thermal stability of the Al70Ni10Ti10Zr5Ta5 amorphous alloy powder fabricated by mechanical alloying’ by Xiu Wei, Xinfu Wang, Fusheng Han, Haowen Xie, Cui’e Wen, J. Alloys Compd. 496 (2010) 313–316
  55. Influence of Mechanical Activation on Decomposition of Titanium Hydride
  56. Production, Kinetic Study and Properties of Fe-Based Glass and Its Composites
  57. Al-based metal matrix composites reinforced with nanocrystalline Al-Ti-Ni particles
  58. Crystallization behavior and consolidation of gas-atomized Al84Gd6Ni7Co3 glassy powder
  59. Crystallization kinetics of Zr65Ag5Cu12.5Ni10Al7.5 glassy powders produced by ball milling of pre-alloyed ingots
  60. Crystallization kinetics and consolidation of mechanically alloyed Al70Y16Ni10Co4 glassy powders
  61. Mechanical properties of Al-based metal matrix composites reinforced with Zr-based glassy particles produced by powder metallurgy